255.Heiple C. R., Roper G. R. Mechanism for minor element effect on GTA fusion zone geometry // Weld. J.— 1982.— N 4.— P. 97s— 102s. 256.Hinchfeld G., Weinschenk H.-E. Spektrogra-phische temperatux bestimmung on Schweiss-lichtbogen // Schweisstechnik (DDR).— I960.— 10, N 12.— S. 438—447. 257.Hnwden D. Mass transfer of metal vapour and anod temperatures in arc welding // Weld. J.— 1966.— N 3.— P. 125—132. 258.Hummitzsch W., Zollenkopf H Die elektrische Leitfähigkeit der Umhüllungen und Schlaken von Schweisselektroden // Schweiss. und Schneid.— 1964.— N 2.— S. 45—50. 259.Ishizaki K., Oishi A., Kumagai R. A method of evaluating metal transfer characteristics of welding electrodes // Phys. the welding Arc: Sympos.— London, 1966.— P. 148— 155. 260.Ishizaki K., Oishi A., Kumagai R. On the Metal Transferring Characteristics of Welding Electrode//J. Jap. Weld. Soc— 1963.— N 3.—P. 187—191. 261.Jelmorini J., Tichelaar G. W., VandenHeu-velG. J. P. M. Droplet temperature measurements in arc welding//IIW-document.— 1977.— N 212—411. 262.Jenkins N. Met A., Moreton J. etat. II Welding Fume, vol. 1. Published by the Welding Inst., Abington Hall Abington.— Cambridge CB16AL, 1981.— 219 p. 263.Jenkins N. Met A., Moreton J. etal. Welding Fume, vol. 2. Published by the Welding Inst., Abington Hall Abington.— Cambridge CB16AL, 1981.—P. 211—506. 264.Jüttner B. Erosion craters and arc cathode spots in vacuum // Beitr. Plasmaphys.— 1979.— 19, N 1.—P. 25—48 265.Keen B. J., Mills K. C, Bryant J. W., Hondo's E. D. Effect of interaction between surface active elements on the surface tension of iron // Can. Met. Quart.— 1982.— N 4.— P. 393—403. 266.Keyte J. B. Influence of the power characteristics under the direct current welding// Weld. J.— 1951.— 30, N 12.—P. 1079— 1083. 267.Kimura Y., Ichihara I., Kobayashi M. Some quantitative evaluation of fumes generated from coated arc electrodes // IIW Doc. II-701—74.— P. 17. 268.Kimura S., Kobayashi M., Godai T., Mina-to S. Investigation on Chromium in Stainless Steel Welding Fumes//IIW Doc. II-E-286—79. 269.Kobayashi M., Maki S., Hashimoto Y., Su-ga T. Some considerations about the formation mechanisms of welding fume // Weld. World.— 1978.— 16, N 11/12.—P. 238— 245. 270.Kobayashi M., Maki S., Ohe 1. Factors affecting the amount of fumes generated by manual metal arc welding V IIW Doc. II-E-211—76.—P. 22. 271.Koves A. Analysis of C02 welding process of thin plates//IIS/IIW Doc. XII-909—85.— P. II. 272.Kubono T. The evaporation rate from a single cathode spot on precious metal electrodes in vacuum arcs//J. Appl. Phys.— 1979.— 50. N 12.— P. 7958—7964. 273.Lancaster J. E. Influence of Heat flow on Metal Transfer in Metal Transfer in Metal Inert Gas Welding of Aluminium // Physics of the Welding Arc : Sympos.— London, 1966.— P. 126. 274.Langmuir I. The interaction of electron and positive ion space charges in cathode sheaths // Phys. Rev.— 1929.— 33, N 6.— P. 954—957. 275.Lee Т. H., Greenwood A. Theory for the cathode mechanism in metal vapour arcs // J. Appl. Phys.— 1961.— 32, N 5.— P. 916— 923. 276.Lesnewich A. Control of Melting Rate and Metal Transfer in Gas-Shielded Metal — Arc Welding. Part 1 // Weld. Research Supplement.— 1958.— N 8.— P. 343s—353s; Part 2 // Ibid.— 1958.— N 9 — P. 418s— 425s. 277.Lesnewich A. Electrode activation for inert — gas — shielded metal arc welding // Weld. J.— 1955.— 34, N 12.—P. 1167—1178. 278.Lucas W. Computers in arc Welding : The next industrial revolution. Part 3 : Instrumentation and process analysis // Met. Constr.— 1985.— N 7.— P. 431—436. 279.Mackeowen S. S. The cathode drop in an electric arc//Phys. Rev.— 1929.— 34, N 4.— P. 611—614. 280.Magnusson E. J., Rosendahl С. H. Studies of the possibilities of classifying welding electrodes according to fume generation. IIW Colloqium on «Welding and Health // IIW Doc. II-E-301—80. 281.MathiasD. L. Recent Development on Contact Electrodes//Weld. J.— 1955.—N 4. S. 316—328. 282.McMasterR.C, MartinD.C, LeathermanA. Analysing Metal Transfer in Arc Welding // Weld. J.— 1949.—N 12.—P. 575s—583s. 283.Mijasaka K., Oshiba F., Akamatsu T. Effect of Eccentrisity of the Coating upon the Deposition of Weld Metal 1/3. Jap. Weld. Soc— 1982.— N 7.— P. 47—55. 284.Moreton J. Welding Fume/ Welding Inst., Abington Hall Abington Cambridge CB16AL, 1983.— Vol. 3.— 113 p. 285.Morita N. Tanigaki T. Investigation on welding fumes from covered electrode and development of low fume electrodes // IIW Doc. 11-818—77. 286.Muller A., Green W. G. Rothschild G. R. Characteristics of Inert-Gas-Shielded Metal-Arcs//Weld. J.—1951.—N 8.—P. 717— 727. 287.Needham J. C. New-generation meters track weld parameters // Weld. Des. and Fabr.— 1980.— N 10.— P. 70—74. 288.Nurnburg A. W., Bauder U. H., Mooser C, Behrisch R. Cathode erosion in vacuum arcs
Карта
|